Current Position:首页 > Products > Pre-processing

Softening

TIME:2014-10-31 10:10:30FROM: AUTHOR:
Softening of preparing for corn germ oil head working procedure.In this process, make the corn germ in heat treatment of the moisture content is below 10% at th...

Softening of preparing for corn germ oil head working procedure.In this process, make the corn germ in heat treatment of the moisture content is below 10% at the same time, make the material embryogenesis plastic changes.

             调质工段Conditioning-section.jpg
Soften the commonly used hot air dryer or heat steam roller dryer, should not be when material embryo in the softening temperature, rapid, in order to prevent the premature protein denaturation and make the material embryo lose elasticity, then affects flaking, steaming and frying, and oil processing.


PRE:Cleanup